Automatic paper lid machine is manufactured by introducing advanced   molding process besides perfecting traditional molding crafts. So it is   characterized by high stability, high productivity, low energy   consumption, little raw material depletion, simple operation and easy   maintenance. What's more, automatic paper lid machine enables one person   to manipulate several machines at the same time, thus liberating labor force.

Automatic Paper Lid Machine Technical Parameters  

<-------- Can Move Left or Right -------->
ModelZGJ-60
Raw MaterialPE coated paper, suitable for 250-380gsm
Cover Diameter65-125 mm
Speed≤40 pcs/min
Power Source220V/380V 50HZ
Power6.5KW
Weight2600Kg
Packing size(L*W*H)2380*1600*1900mm
Air pressure requestWorking pressure: 0.4Mpa, Working air flow: 0.12m3/min